Good price  online

products details

Created with Pixso. Home Created with Pixso. Products Created with Pixso.
Zinc Plating Additives
Created with Pixso. DS-515 Low Concentration Acid Chloride Zinc Plating Process Without Boric Acid Ammonium

DS-515 Low Concentration Acid Chloride Zinc Plating Process Without Boric Acid Ammonium

Model Number: DS-515
MOQ: 25-30kg
Delivery Time: 5-8 work day
Payment Terms: T/T
Detail Information
Place of Origin:
China
Product Code:
DS-515
Type:
Low-Concentration Acid Chloride Zinc
Potassium Chloride:
120-150 G/L
Zinc Chloride:
30-40 G/L
Boric Acid:
25-30 G/L
PH Value:
4.8-6.2
Operating Temperature:
10-50 ℃
Cathode Current Density:
0.5-5 A/dm²
Packaging Details:
25kg/drum
Highlight:

Low Concentration Zinc Plating Process

,

Acid Zinc Plating Process

Product Description

DS-515 Ultra-Low Concentration Acid Chloride Zinc Plating Process Acid Bath Without Boric Acid Or Ammonium

Performance & Features

RG-515 brightener is an acid chloride zinc plating technology that produces highly ductile and well-leveled coatings under a wide operating window, compatible with both rack plating and barrel plating. It features innovative technical indicators in resource utilization, energy conservation, consumption reduction and emission reduction.

  • No cloud point
  • High temperature resistance
  • Wide operating temperature range
  • Energy-saving & emission-reducing
  • Fast deposition rate
  • Excellent leveling performance
  • Ultra-low working concentration
  • High cost performance
Operating Parameters
Item Concentration / Range
Potassium Chloride (KCl) 120–150 g/L
Zinc Chloride (ZnCl₂) 30–40 g/L
Boric Acid (H₃BO₃) 25–30 g/L
RG-515 Brightener 0.1–0.5 mL/L
RG-515 Softener 20–30 mL/L
RG-515 Auxiliary Agent 6–12 mL/L
pH Value 4.8–6.2
Cathode Current Density 0.5–5 A/dm²
Voltage (Rack Plating) 3–8 V
Voltage (Barrel Plating) 6–12 V
Operating Temperature 10–50 ℃

Acid bath without boric acid or ammonium
The coating has high corrosion resistance
Easy to manage tank fluid
Low foaming type, excellent coating appearance can also be obtained under high temperature conditions
Meets environmental requirements such as ROHS.ELV